Basic Finishing
- Deburring — Manual, vibratory, thermal, CNC
- Cleaning — Ultrasonic, solvent, drying
- Basic Polishing — Surface preparation
- Sandblasting — Surface texturing
- Brushing — Directional finish
- Inspection — Coating thickness & adhesion check
Anodizing, Plating, Coating, Heat Treatment and More
Comprehensive surface finishing through in-house processes and qualified treatment partners. From anodizing and plating to powder coating and heat treatment — ensuring parts meet functional, cosmetic and corrosion-resistance requirements.
Basic finishing is completed in-house. Specialty treatments are managed through qualified partners under our quality system.
Available on finished surfaces for branding, identification and traceability.
Different materials require different surface treatments. Here is what we provide for each material group.

























Key performance data for common surface treatments — actual results depend on material, thickness and specification.
| Finish | Thickness | Surface Hardness | Salt Spray | Typical Material |
|---|---|---|---|---|
| Clear/Black/Color Anodizing | 10–25μm | HV 250–350 | 48–168h | Aluminum Alloys |
| Hard Anodizing (Type III) | 25–80μm | HV 400–600 | 336–1000h | Aluminum (6061, 7075) |
| Hard Chrome Plating | 10–50µm | HV 850–1050 | 96–240h | Alloy Steels (40Cr, 42CrMo) |
| Electroless Nickel (ENP) | 5–25µm | HV 500–900 | 72–200h | Steel, Brass, Copper |
| Zinc Plating (Cr3+) | 5–25µm | HV 100–150 | 48–120h | Carbon Steel |
| Passivation | < 0.005µm | Base Metal | 48–96h+ | Stainless (304, 316, 17-4PH) |
| Black Oxide | < 2µm | Base Metal | 24–48h | Tool & Carbon Steels |
| QPQ / Liquid Nitriding | 10–20µm | HV 700–1000 | 200–500h+ | Carbon & Alloy Steel |
| Carburizing & Quenching | 0.5–2.0mm (Depth) | HRC 58–62 | — | Low Carbon Alloy (20CrMnTi) |
| Gas / Ion Nitriding | 0.2–0.5mm | HV 750–1100 | 48–96h | Alloy Steels (38CrMoAl) |
| Gold / Silver Plating | 0.5–3µm | HV 150–200 | 24–48h | Copper & Brass |
| Powder Coating | 60–120µm | 2H–4H | 300–1000h+ | Steel, Aluminum, Sheet Metal |
Salt spray hours and hardness values are typical ranges. Actual performance depends on material grade, thickness, process parameters and specification.
Deburring, cleaning, basic polishing, sandblasting, brushing and inspection are in-house. Anodizing, plating, coating, heat treatment and specialty finishes are managed through qualified treatment partners under our quality system.
From 24 hours (black oxide) to 1000 hours (powder coating). QPQ/Melonite achieves 200+ hours with HV 500–700 surface hardness. Specific resistance depends on the finish, material and specification.
Yes. Hard anodizing achieves surface hardness HV 400–600 with thickness 25–80μm. Clear, black and color anodizing are also available.
Yes. Quenching, carburizing and nitriding are available through qualified heat treatment partners, coordinated under our quality system.
Yes. Coating thickness measurement and salt spray test reports can be provided per customer requirements.
Send us your drawing with surface finish specifications (finish type, thickness, color, salt spray hours). Our team will coordinate the full finishing chain.